Thanks Ed and Chumpes,
but is there a relation between nickel and chloride ? what is the main factor so that 42% Ni are immune ? is there a passivation layer ? nickel chloride solubility ? FCC structure ?
Please help
Experts,
What is the relation between Austenitic & Nickel alloys in term of Intern-granular corrosion and Chloride Stress Corrosion Cracking ?
Why these mechanism occurs only in these specific alloys ?