Hello there. due to the repeated failures (abbrasion) of high sch carbon steel lines (4 to 6 in), i have been asked to propose most suitable piping for this process which is crushed salt disolved in water along with sand... as slurry. I came cross some prevous proposals of CS rubber lined, pp...
Hi all,
I am not sure this is the right place to post my question or not.
We are going to revamp plant to new technology with slight increase in capacity.
Some equipment such as columns, tanks, heat exchangers...will be reused and few will be repurposed.
Is there any systemic approach to conduct...
Thanks Ed. I did some investigation and found that the pH is 2 and occasionally can reach 1.5. Looks Ti Gr 12 may not survive and what about Gr 16?
thanks
Hi glad to be member of this Forum.
Ti Gr12 has been used to construct pressure vessel to contain water contaminated with chlorine and some salt traces. Ti Gr 12 is potential of having crevice and pitting corrosion after 70 Deg. C. any suggestion of alternative or special care?