Hi there,
as per my experience, weldolet thickness should be same as the pipe thickness as specified in piping class. for example
20 in is sch 40
1 in is sch 160
20 in X 1 in weldolet should have sch 40 X sch 160 in its description. you can always accept higher thickness and machine to...
Hi all and thanks in advance for your participation
regarding nozzle loads on rotating equipment's, we are following the rule of thumb: twice the values in API 610 table 5.
any reason for this rule ?
are you guys using it ? or you follow other standard ?
pump spec API610
piping spec. B31.3...
dear friends
i am working for a client following shell standard, so we use predefined piping classes and all components have a ready data sheet.