How close is your UTS to the min required?
(UTS achived is 772 MPa against min. required of 760 Mpa.)
Typically tempering at higher temperatures will achieve this.
(Temped twice first at 620 deg. Cent. and second at 575 deg. Cent.)
I presume that this material is being quenched and...
Hello Experts!
We are producing Gx4CrNi13 (1.4317) with following composition:-
C = 0.013 %, Si = 0.41 %, Mn = 0.47 %, P = 0.027 %, S = 0.0062 %, Cr = 12.33 %, Ni = 4.71 %, Mo = 0.422 %, Al = 0.046 %, Cu = 0.181 %, Co = 0.0017 %, Ti = 0.005 %, V = 0.011 %, W = 0.032 %, Pb = 0.002...