    Hi , we are developing the blister

    Yes , it covered with peelable aluminum foil. It's Europe .
  2. StG10

    Hi , we are developing the blister

    John2025 , The mechanical design is ours. The blister is not simple , it suits for robot gripping has magnet switch and some other features that worse to design inside the company . Blister's producer(thermoforming plant) suggested pETG ,than GAG and we had problem with that and meanwhile have...
  3. StG10

    Hi , we are developing the blister

    btrueblood , Yes i reviewed it , but aluminized pvdc sheets are not translucent . Regarding Aclar , their site suggests maximum thickness of 7.8 Mil and sale it sheets 8”x 10” ,that is too small . I'm trying to contact them .
  4. StG10

    Hi , we are developing the blister

    Hi , we are developing the blister for medical device that can be produced by means of vacuum forming. We tried PETG or GAG materials type. The problem -the product doesn't withstand moisture test ,caused by high glycol level in PETG/GAG ,meaning the blister pass too much water during humidity...
  5. StG10

    Material for Vacuum formed blister

    Thanks for the information and link . I haven't found information whether PVDC can be used in Plastic Vacuum Forming. can you advise ?
  6. StG10

    Material for Vacuum formed blister

    It means the bag pass too much water during humidity testing. Can you please advise any brand of PVDC that that besides of less moisture permeability has dielectric strength and translucent appearance?
  7. StG10

    Material for Vacuum formed blister

    thread108-216193 Hi , we are producing blister for medical device by means of vacuum forming. The materials are PETG or GAG . The problem -the product doesn't withstand moisture test ,caused by high glycol level in PETG/GAG and we are looking for alternative material ,that is suitable for...