This was the answer I was looking for. Thank you very much. I presented my client with this solution before, but it was immediately rejected. I wanted further clarification before a second attempt into the lair.
Thanks again.
Thanks for the response, but I do not want to clad the weldolet as it is solid Inconel. I must drill a hole in the wall of the main process pipe to allow for the instrument connection. I must ensure that the CS outer section of the process pipe, which is now open to process gas as I have...
I have a substantial amount of Inconel clad CS piping ranging from 8" - 32". The average WT of the CS is 19mm, with a 3mm thick Inconel cladding. My problem is that I have numerous 3/4" instrument connections that require weldolet or weldoflange connections. I must ensure that...