  1. BHagood

    AMS 2770, Aging 7075-T6 to T76

    To be more clear. I'm trying to understand if the material has to have solution heat treatment again or just go through the aging treatment.
  2. BHagood

    AMS 2770, Aging 7075-T6 to T76

    Needing confirmation on the process to age some 7075-T6 sheet to T76. It looks like since material is already T6 temper, per table 7 of AMS 2770 it would just require 16-18hrs at 325 degrees. Is this correct?