    NDE of a non-pressure boundary weld

    No loading on the cone, it can be thought of as simply directing the flow, almost as a flow conditioner. The only pressure the cone would be subject to is from the fluid, and since it is fully surrounded the net pressure is 0, AFAIK. We perform 100% visual examination, the issue is when PT or...
  2. accordigang

    NDE of a non-pressure boundary weld

    Hello all, we have been having a discussion about completing NDE on welds that are not on a pressure boundary. I've tried looking online for similar examples and through our ASME codes (B31.1 most often) but have not found anything. In our example, we would have a welded cone that is fixed and...