    chromic acid anodize per stp 58-209, ty i and br 127

    Hi Sparweb, Yes, you are correct. Sequentially is what I meant. It's all a very large learning curve for me at this time. I am taking in all the information that I am finding on this forum. I am so grateful for all this provided information. I believe due to our contract that is why are are...
  2. _LynseyJames

    chromic acid anodize per stp 58-209, ty i and br 127

    Hi WKTaylor, Thank you so much for the reply, I am looking into the 'light reading' as we speak.
  3. _LynseyJames

    chromic acid anodize per stp 58-209, ty i and br 127

    Hi Sparweb, thank you for the reply.. We're not able to find a company that can perform the two processes together. For myself, I am one month into working for Topflight, my background is not aerospace. Thank you again for taking the time.
  4. _LynseyJames

    chromic acid anodize per stp 58-209, ty i and br 127

    Hi, I'm very new to this business. Does anyone have any experience with companies that have the capability to process 7075-T6 Bare sheet metal with Chromic acid anodize per STP 58-209, Ty I and BR 127? TIA, Lynsey