    Need to improve Charpy Results

    Hi Guys. I need your advice. I am current working on a NiCrMo material which the mechanical property requires a 30J at 20c. This material has 3 stage of heat treatment which are Normalise@980c Harden@930c and temper at 210c. For now i only can archive a min 25 to max 28J. Can you please advice...