    17-7PH

    I have 1 part need to use 17-7PH and do treatment of H1025. However, after machining very hard to control with this treatment and thus supplier propose to use pre heated material 17-4PH which comes along with H1025. Is it possible? Do I need to check if the HRC of using 17-4PH is same as using...