In hypoeutectic foundry alloys (Al-Si), which A356 falls in, copper is added to improve tensile strength, machinability and thermal conductivity. However, this increase is at the expense of a reduction in ductility and corrosion resistance.
At 0.42% Cu instead of <0.2%, you might expect lower...