arunmrao
Thank you for the response...I have used 410 for wear plate in controlled environments with excellent results. My concern with SA240-410 in this application is the high carbon content in reaction to the PH and corrosion from oxidation. Can you lend any advice regarding my concerns...
TVP
Thanks for the info...funny thing is that I have done so much work for AK Steel Middletown and Ashland plants that you would think that I would have immediately thought of Nitronic 30. It totally slipped my mind...As a matter of fact I have convinced many of their maintenance eng. to move...
I have a customer that hauls light weight aggregate materials to construction sites across the midwest. This aggregate develops a Ph of 14+ when wet. We would normally use Hardox from SSAB to line haulers. I do not believe that Hardox will stand up to the Ph levels. He asked me if building a...
I have a customer that hauls light weight aggregate materials to construction sites across the midwest. This aggregate develops a Ph of 14+ when wet. We would normally use Hardox from SSAB to line haulers. I do not believe that Hardox will stand up to the Ph levels. He asked me if building a...
It should be appropriate to use Teflon gasket and bolt material of ASTM 193 B7.
Timothy C. Odom, CEO
Odom Industries, LLC