Hi,
can some body help me?I need a soluble (hexane,heptane) but pre-vulcanized (only minor crosslinked/or not crosslinked would be even better) SBR rubber or other similar rubber type.Is there some company offering these polymer-additives?
thanks lots for helping
have a nice day
sincerely
Tim
Hi JStephen,
thanks for your answer and help. I thought of reducing generated combustion temperature...nice to be understood even when things not clear :).
I just had in mind of treating heat sensitive materials like plastics and stuff. So at least the max temperature should be in this range...
Hi,
is there a way to obtain a flame temperature of gases with lets say 300-600°C [ponder]? I found out alkanes for ex. butane, propane have a much lower combustile temperature than oxygene related. Can a gas be mixed with some sort of chemical to keep it that low on heat?
thanx for help
Timmy
Hello community,
i am trying to find a way of applicate a rubber-resin
pressure sensitive hotmelt. I have read many literature about TEAS graphs and solvent mixing solutions (15% high boiling - 85% low boiling solvents) and hotmelt application
and tried many mixes. All has not worked :(. I need...