Is there any purpose to passivating inconel 718 springs? The springs are used in an aerospace application, therefore the corrosion resistance requirements are high.
Would electropolishing be a better option?
I have a question regarding welding two 316L (ASTM A479) parts together that have different hardness and slightly different chemical compositions.
The first has a UTS of 110ksi, yield of 75ksi.
Chemical Comp: C .014%, Si .62, Mn 1.37, P .027, S .017, Cr 16.83, Mo 2.01, Ni 11.14, Ti .125, Co...
Yes. I've looked at Carr Lane, McMaster-Carr (of course!) and Vlier, among others. All offer varying types of spring plunger, however none have a plunger that extends through the body.
I am looking for a spring plunger I can use to indicate a part is fully seated inro a hand tool. Therefore the plunger nose will have to go through the body and extend out the other side when the spring is fully compressed.
I am looking for a 10-32 thread plunger, with a spring constant of...