  1. soundbite64

    17-7 PH SS

    Is there a procedure to repair the parts that I have or are they scrap? Do I need to have the sheet supplied in condition C?
  2. soundbite64

    17-7 PH SS

    Thank you for the help. Yes the material is magnetic, and I have ask for the COT from my supplier. Prior to heat treating the material had a hardness of B82.
  3. soundbite64

    17-7 PH SS

    I have made some retaining clips from 17-7 PH SS and have had them heat treated for one hour at 900F for what should be CH900 but the material has become very soft (rockwell C8). These parts were made from 0.071 sheet stock that has the 17-7 stamped on it from the mill. Why is the material so soft?