I have specified Ra 0,2 um on some PEEK sealing surfaces. This is not achieavable by milling, only by polishing. This is a time-consuming operation that could increase cost a lot. You could also try heat treatment using the same 'lighter trick' normally used on scratched CDs, but PEEK has a much...