    You may try PPS + 15%carbon fiber + 10% PTFE + 2% PEEK. We do some experiment (not for oxygen services) by compare above formula with 10%carbon fiber 10%PTFE 10%GRAPHITE 70%POLYETHERETHERKETONE. PPS base material show better performance at 60 DEG C. *PPS is very low cost.