    Aluminum Molds

    mjh368, glass is already 30%, can't go much higher! Mike, I just might try that. Never seen a hot water dip before. The other idea I have is to also inject gas into the part. I'm not too concerned about voids as the part isn't structural and this may also give me reduced cycle times and better...
  2. mdg123

    Aluminum Molds

    Excuse me for jumping in, but this is the closest thread I've found to what I'm looking for. I'm running a very thick inj molded PP+30%glass part and having sinkage problems. I have a lot of experience molding with Nylon+glass and have found a sizable gate, hot mold, and hard and fast shot to...