  1. polina

    Hot Fluid Bad

    Our company is using hot fluid bed or hot sand bath to clean the screws and other parts from hard plastic from extrusion or injection molding. Right now we send out parts to a bigger plant and a lot of it gets lost in a large sand bath. I am looking into buying a hot sand bath that would be...
  2. polina

    cleaning injection mold screws & barrels

    At my company we use hot sand bath or hot fluid bad were we submearch the screw an other parts for regular clean up.