  1. happychemist

    question about coupling unlike metals

    Is it an open-loop process, or is it a pure closed process ? In the second case, You may have problem with hot caustic with Fe traces due to your bag filter; Fe traces may cause corrosion "pitting like" on austenitic ss, in particular on cold worked (eg. swifting elbow), parts without...