  1. metallurgicalman

    ASTM G48-A

    Mr Ed All good questions but I have few answers! This is the test result as reported on the MRC. As the test is ASTM G48 - A, I assume that the test-piece was 50mm x 25mm x unknown t and prepared according to G48. Temperature was 30ºC, duration 24 hours.
  2. metallurgicalman

    ASTM G48-A

    Would anyone consider 0.2g/m2 weight loss acceptable for 31803 (no pitting observed)? Sounds a bit high to me!