    high silicon - flash-butt welding

    metengr, Thanks for your reply. Yes You are right, but I didn't write that this steel doesn't exist. It is only a development project. So I can try to image a pull test of this steel, but without any results. So, as well as Thanks
  2. lukkaa

    high silicon - flash-butt welding

    Hello, I would like to ask you for your opinion. I have a high strength low alloy steel (0,2-0,25% C, Ni,Mo,Cr) with addition of silicon (about 1,3%). This steel is welded with flash-butt welding and carbon equivalent is satisfactory for this type of welding. But I have read that silicon over...
  3. lukkaa

    Boron steel - welding

    Hello, I would like to ask you for your opinion. I have a high strength low alloy chain steel (0,2-0,25% C, 1% Ni, 0,5% Mo, 0,5%Cr) with addition of boron (0,002-0,0035%). For the suppression of boron nitride precipitation is this steel sufficiently titan treated (nitrogen about 0,006%). So...
  4. lukkaa

    Hadfield steel

    Hello, I have a chain consists of weld joint of hadfield steel and Cr-Mo-Ni steel. I would like to carburize this material (900-920°C). Next process will be a quenching (840 - 860°C/water) and a tempering (180-200°C). What do you think, is it possible to do it without cracks or lowering the...