tjrush2000
Just finished having to deal with the Japanese with Q-235 mat'l verses A36 mat'l
The only option was to run mat'l through the series of qualify procedures, Charpy, NDT, etc... to ensure that it met A 36 standards.
Your trying to ensure 304L will meet US Std, so plan on doing the...
Mr168,
Thanks for the post.
I am curious about Q 235 falling under P1 Material? if this is correct, then our WPSs/PQRs using Group P2 to P2 would also qualify Q 235 if it is a Group P1 Mat'l, Yes/No?
Thanks again for the update
What is going on with this Asian crap! anyway
I am experiencing the same issues read in your previous forum on Q 235 material. Jusr received a call from client in Martinsburg, W. Virginia regarding welds completed on Q 235 material were cracking and the supplier has no answers and not willing to...