  1. kjsn24

    Normalizing Anneled Material

    No, the part process does not call out post weld normalizing. The notes specify using normalized material.
  2. kjsn24

    Normalizing Anneled Material

    We have a part that calls out to use 4130 Normalized .050" thick sheet metal per AMS 6350. The part is formed into a tube and MIG welded at the seam. Would there be any issues if we used Annealed material (.050" 4130 AMS 6350) and Normalized it after forming and welding?