Yes, you can also view it in that way.
1% offset yield strength is obtained by moving in the strain (x) 1% and draw a parallel line from the elastic range.
Normally is used 0.2%
My question is, what is the criteria to use 1% offset yield strength? (more that the ovious higher yield value)
thread794-467405
Good morning Eng Comunity.
I would like to know in which case is possible to use 1,0 % proof strength in the design thinkness of a tank.
Kind regards,
thread794-501203
Dear All,
I hope this thread finds you well.
I have a question regarding the necessity of performing a Fatigue assessment
Currently, I am designing a vessel with the design pressure and temperature of 4 4barg and 80C. Nothing special, but operate in batches a fluid that is...