    17-7 PH Spring Steel forming with heat treatment

    Thanks To all the responders. Cold forming such a shape is cost prohibitive at this stage in terms of cost. I had approached Smiley in the past and although their customer support is excellent, this is outside their normal process enough that they cannot do it Here is what I am thinking now...
  2. SABAS

    17-7 PH Spring Steel forming with heat treatment

    I am on a project where we are using 17-7 Condition C (Cold Rolled) The strips are either 0.012" or 0.008" thick and ~1/4" wide We need to form these into a radius of proximately 6" radius and 4" radius (in actuality it is not a perfect arc but this gives an idea of the curve required We...