Ed, Thanks for the info. What do you mean by "long soak" at 600F? Alloy digest says 1hr, should I go longer?
On the 400F to -100C cycles, should I be concerned about ramp rates and soak time at high/low set points?
Thanks,
Chris
I designed two optical mounts out of Invar 36 and had them machined with no heat treating. They are basically 1/2" thick plates 4" x 6" with a bunch of pockets that each hold a 3" diam mirror.
After aligning at room temp, we lose alignment when we run the assembly down to operating temp of...