  1. RNDROB

    Need help selecting a suitable material.

    Thank you all for the continued ideas, all good stuff. Why the male part is H900 I don’t know. It has been since initial design in 1993 and the people involved are not longer around. I have a very reasonable quote for the Nitronic 60 and will probably go that way.
  2. RNDROB

    Need help selecting a suitable material.

    Thanks for the reply. Can you explain your comment about 17-4 heat treat at h1100 rather than h900? Thank you,
  3. RNDROB

    Need help selecting a suitable material.

    I have a mechanism in an assembly that is causing a problem and I need some suggestions. The application is on the wet end of a paper making machine. Chemical environment is typically alkaline. We prefer to use 316 SS when we can. 316SS has a tendency to gaul when used for threads. We have...