  1. AleksandarLPO

    Pull rods for creep test

    Finally I will make shells and cast bars myself. Machining should not be a problem!
  2. AleksandarLPO

    Pull rods for creep test

    Still did not found anyone who can and will produce these pull rods. [sad]
  3. AleksandarLPO

    Pull rods for creep test

    Thank you, I tried with them they have to reply to me are they willing, or can, make different diameter than they have on stock. Any other supplier if you can think of?
  4. AleksandarLPO

    Pull rods for creep test

    Hello all, I need help to find supplier for new pull rods for creep testing device. Material is MAR M246. Best Rgards
  5. AleksandarLPO

    Pickling stains

    Well, I am not sure.
  6. AleksandarLPO

    Pickling stains

    No pickle is room temperature, alkaline cleaner is hot
  7. AleksandarLPO

    Pickling stains

    Thanks for help and answers. HNO3 concentration is arround 103g/dm3 HF is arround 2.7g/dm3. part has to look good.
  8. AleksandarLPO

    Pickling stains

    Well, after sandblast, degrease in trichloroethylene, then cleaning in Turco and finally pickle in HNO3+HF bath.
  9. AleksandarLPO

    Pickling stains

    Hello all, we are performing pickling on greek ascolloy castings and on some parts on some batches we got stains, 3-4 hundrets of milimeter high, very difficult to remove. Is there any idea what it came from, what is the problem? Thanks