Jan 27, 2005 #1 pt1000 Mechanical Jan 14, 2005 9 0 0 DE Does anyone know if 1,3 pentadieen is corrosive on GRP for tanks or FPM on pumpbellows. Concentration is <1%,
Does anyone know if 1,3 pentadieen is corrosive on GRP for tanks or FPM on pumpbellows. Concentration is <1%,
Jan 28, 2005 #2 25362 Chemical Jan 5, 2003 4,826 0 0 CA Why should pentadiene attack glass-reinforced plastics or flurocarbon rubbers ? At what operating conditions ? In what solvents is the 1-methyl butadiene dissolved ? Upvote 0 Downvote
Why should pentadiene attack glass-reinforced plastics or flurocarbon rubbers ? At what operating conditions ? In what solvents is the 1-methyl butadiene dissolved ?
Feb 4, 2005 Thread starter #3 pt1000 Mechanical Jan 14, 2005 9 0 0 DE Why it should attack? I don't know, that's why I started this thread. The solvent is Aluminum Chloride 7%, conditions are atmosferic pressure and ambient temp. Upvote 0 Downvote
Why it should attack? I don't know, that's why I started this thread. The solvent is Aluminum Chloride 7%, conditions are atmosferic pressure and ambient temp.
Feb 4, 2005 #4 StoneCold Chemical Mar 11, 2003 992 0 0 US pt1000 You are still missing 92% of your material composition. Upvote 0 Downvote
Feb 14, 2005 Thread starter #5 pt1000 Mechanical Jan 14, 2005 9 0 0 DE Sorry, thought it was obvious, 92% water Upvote 0 Downvote