Jun 21, 2018 #1 hawkaz Structural Oct 28, 2010 409 US Can a CJP weld be done with this steel? Tube to tube or tube to plate. Thanks
Jun 21, 2018 #2 EngineerTex Mechanical Apr 17, 2008 368 US Why couldn't it? Do you have a WPS for a CJP for this thickness to be welded from one side? Engineering is not the science behind building. It is the science behind not building. Upvote 0 Downvote
Why couldn't it? Do you have a WPS for a CJP for this thickness to be welded from one side? Engineering is not the science behind building. It is the science behind not building.