300M, EN30B AND VascoJet 1000 for crankshafts

Status
Not open for further replies.

Paulie

Mechanical
Oct 17, 2001
2
Can anyone give any information regarding the suitability of 300M, EN30B and VascoJet 1000 (any or all of these) for crankshaft applications. I undestand EN30B is used but is there anything better? (must be ferrous)
Any help appreciated!
 