304 stainless steel vs Potash (Potassium Chloride)

Status
Not open for further replies.

actionpaxt

Mechanical
Jun 24, 1999
3
how does 304 ss hold up to a 316 ss or an alloy when in contact with potash that is frequently washed down?
 
Replies continue below

Recommended for you

The Shell Corrosion Data Survey doesn't show any difference in the two.
 