Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

310 SS for CO2 & H2S Content Hydrocarbon Gases 1

Status
Not open for further replies.

masi

Mechanical
Nov 12, 2001
1

Can we use 310 SS material for a hydrocarbon gas with 8% CO2 and 8% H2S and 2% H2O. Gas temp: 80 degree C.

Thanks.
 
Replies continue below

Recommended for you

If your water dew point is below 80C Carbon steel should be suitable. Unsure of your application, if corrosion is an issue, 304 or 316 grades should be suitable at that temperature. 310 is typically utilized in higher temperature applications.

Regards
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor