I wud like know about the resistence of SS 316l in dilute sulphuric acid(4%) &caustic soda(44%) service? I m talking about a waste whose Ph varies anywhere in between 1 to 14 where this material is going to be used. Can anybody answer in detail plz.

I know that austenitic ss cannot withstand chlorides, so if its not HCl but H2SO4, will it be OK?
 
Replies continue below

Recommended for you

316L is recommended for both at ambiant temperatures, meaning less than 0.1g/day per meter square. 316 is a good storage container for such solutions.
 