I am currently using Asiga Max UV 3D printer for my prototyping of model. The material used for printing is Asiga PlasCLEAR. The part colour is changing to light yellow after print is completed. Any reasons for this.?
Thank you!
I'm not sure if you meant to post this in the structural engineering discussion forum, but you might better be served in a 3D printer hobbyist forum, or in the mechanical engineering discussion forum where they'd be more likely to use 3D printing.