Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

500W IPG fiber laser cutting of 4mm SS with oxygen

Status
Not open for further replies.

ciraq

Industrial
Mar 11, 2015
1

Hi..

I am new user of 500W IPG fiber laser, I am facing problem of lots of dross at bottom side while cutting 4mm SS304 with oxygen.

I am using pre-set cutting data but its not helping much.. using speed 1m/min, power 500watt, freq. 20,000Hz, using 5" lens, 2mm nozzle and gas pressure 4bar. During cutting...melted parts stick to bottom surface and its very hard to remove it. when I asked to machine supplier they said that SS cutting with oxygen has this default characteristic!

Some of our competitor having similar power laser machine and they are having clean cut! its really disappointing to loose business because of bad cutting quality.

If existing user can help me out?? welcome for your comments!!

 