Oct 23, 2006 #1 Roachman Automotive Jun 17, 2003 13 0 0 GB Could anyone provide me with basic properties such as tensile strength etc for 50MnT steel which is the material used for a gear I am about to use?
Could anyone provide me with basic properties such as tensile strength etc for 50MnT steel which is the material used for a gear I am about to use?
Oct 24, 2006 #2 MOB1 Materials Feb 11, 2003 69 0 0 AU Are you sure that the steel's designation is not 50Mn7? 50Mn7 is a standard German steel somewhat like AISI1552 but with manganese in the range 1.60-2.00%. Upvote 0 Downvote
Are you sure that the steel's designation is not 50Mn7? 50Mn7 is a standard German steel somewhat like AISI1552 but with manganese in the range 1.60-2.00%.