6061-T6 in contact with CF8M Corrosion Concerns

efulm4444

Mechanical
Oct 11, 2022
8
Our assembly has a 6061-T6 component attaching to a CF8M component. The 6061-T6 is anodized per MIL-A-8625, Type II. The connection would be exposed to air on one side and oil on the other. Should we assume there will be galvanic corrosion between the components?
 
Replies continue below

Recommended for you

As long as the air isn't wet there should be no issue. I have seen couplings of bronze and hard anodized aluminum exposed to salt spray and the aluminum did hold up very well. Any defects in the coating and it's fried.
 