1
In my chemical plant, a refractory lined waste heat boiler has developed a hot spot. It is around size of a football and temp. is 300 degC. Can anyone provide information on how to cool this hot spot and continue the plant operation?
 
Replies continue below

Recommended for you

My procedure would be to shut down the boiler and then repair the refractory lining after the furnace has cooled down, otherwise, how could do the job.
 
What's causing the hot spot? Is there a water side problem such that less heat transfer is occurring locally? Has a void developed within the refractory itself?

CR

"As iron sharpens iron, so one person sharpens another." [Proverbs 27:17, NIV]
 
OP doesn't identify the fuel or its firing method, so could be...hadn't thought of incorrect flame shape/geometry.

CR

"As iron sharpens iron, so one person sharpens another." [Proverbs 27:17, NIV]
 
More info would be better, but at first glance a football (round or pointy ends?) sized hot spot at 300°C isn't worth bothering to cool. Continue to run and monitor. Seriously, it isn't all that hot. More of a "warm spot".

Should the spot grow in size or temperature, I'd start with blowing some steam on it to provide cooling. This is very commonly done. Depending on exact circumstances, a sooner than planned shutdown may be in order for a proper refractory or burner repair.
 