A second query on the same subject of Procedure Qualification.

Are the delivery conditions of a plate material taken into consideration while forming the group of materials? For example As Rolled, Controlled Rolled, Normalized, Quenched & Tempered or TMCP steels considered so that there is no need to qualify additional procedures?
 
Replies continue below

Recommended for you

It isn't a variable. Just verify you are qualifying the right material for you production needs. Generally, the material specification will stipulate the rolling practices, state of heat treatment, etc. As rolled would be a different material specification than a quenched and tempered material and are grouped differently.

Best regards - Al
 
Dear gtaw structural,

Thank you very much for your prompt response. The specification was asking for the method of manufacture as an additional essential variable Hence the query.

Regards

S R Ramanujam
 
If you use the material to be used in production for your PQR you will have no problems complying with the requirements of the code and/or your specification.
 