A vs SA for boiler tube

Status
Not open for further replies.

kclim

Materials
Jul 2, 2002
168
Are the SA and A grades for boiler tube interchangeable? In particular, was looking at A/SA-213 and 209.

thread292-209678 seems to suggest for pressure vessels, there is information in ASME II A which details equivalent SA/A grades. Does this apply to boiler tube as well?

Thanks
 
Replies continue below

Recommended for you

kclim;
You need to review ASME B&PV Code, Section II, Introduction. Toward the end of this section is titled Acceptable ASTM Editions. Review this, and discuss with your AI.
 