Hello,
i need thermal expansion coefficients for SA182 F5 material.
ambient up to 1000°F (538°C).
I had a look at the ASME BPVC.II.D - 2017, Subpart 2, Physical Proerties Tables, Table TE-1 but couldtn find 5Cr 1/2 Mo (only 5 Cr 1 Mo) and I am not sure if its an Low Alloy steel of group 1 cause
it is not listed in Group 1 Note 1 or it is more like a 5 Cr 1 Mo.
Thanks!
i need thermal expansion coefficients for SA182 F5 material.
ambient up to 1000°F (538°C).
I had a look at the ASME BPVC.II.D - 2017, Subpart 2, Physical Proerties Tables, Table TE-1 but couldtn find 5Cr 1/2 Mo (only 5 Cr 1 Mo) and I am not sure if its an Low Alloy steel of group 1 cause
it is not listed in Group 1 Note 1 or it is more like a 5 Cr 1 Mo.