Can anyone tell what a good equivalent steel for A194 2HM nut material would be?
Thanks
 
Replies continue below

Recommended for you

Your question is vague. Do you want to know an alloy that meets ASTM A 194 class 2HM properties? Or do you want to know about another standard that is similar to it?

For the former question, a simple steel like SAE 1045 would work.

For the latter question, ISO 898-2 property class 9 is similar but not exact.

Regards,

Cory