Mixel
Materials
- Feb 1, 2007
- 3
Hi,
in order o correctly fill a furnace I need the real value of A357 alooy density when it is melt (2.7 Kg/dm3 is the value for the solid state).
There are some value or some diagram that can shows this phisical quantity?
Thanks,
Michele
PS: I need some info about :
- maximum acceptable value of H2 after degassing of A357 aluminum alloy (? cm3/100g);
- relationship between H2 microporosity and elongation failure on A357 alloy.
Someone can help me?
Thanks a lot
in order o correctly fill a furnace I need the real value of A357 alooy density when it is melt (2.7 Kg/dm3 is the value for the solid state).
There are some value or some diagram that can shows this phisical quantity?
Thanks,
Michele
PS: I need some info about :
- maximum acceptable value of H2 after degassing of A357 aluminum alloy (? cm3/100g);
- relationship between H2 microporosity and elongation failure on A357 alloy.
Someone can help me?
Thanks a lot