78
I need a pipe of 32" A928 Duplex of 8 meter long. My capacity to roll is Max 2m width,so I will be making 4 pipes of longitudinal weld & will weld them circumferetially to each other to make 8 m long pipe.

My question is that will solution anneling will be applicable to cirseam as well?

 
Replies continue below

Recommended for you

What does your client require and what was agreed upon in the contract documents? Talk to them.
ASTM A 928......
17. Lengths
17.1 Circumferentially welded joints of the same quality as
the longitudinal joints shall be permitted by agreement between
the manufacturer and the purchaser.
 