Anybody have temperature knockdown curves I can use for NAS1097AD rivets installed in a high temperature environment (450+ degrees F)?

Previous data where I'm at right now suggest they were only looking at the skin bearing strength.

Thanks in advance,

Joe



--
Great Spirits have always encountered violent opposition from mediocre minds
-- Albert Einstein
 
Try:
Mil-Hdbk-5 (AR-MMPDS-01) Figure 3.2.3.1.2(b)

You won't be too far off...

If they don't buy that argument, can you test coupons while simulating that environment?


Steven Fahey, CET
 
not much data out there on 2117T4; maybe someone has an old MIL-HDBK-5 that has this data. looking at 5J for 2014T6, for 10,000 hrs exposure it looks like Fty falls to 10% and Ftu to 40% (of the room temperature values).
 