May someone have any practical experience or information regarding Arsenical Admiralty Tubes (Alloy UNS No. C-14200)?
To be specific: is the arsenic component dangerous / carcinogenic? In case it is not, does it comply with FDA requirements for food service system?
Does it have any advantage in corrosion resistance in comparison to regular admiralty metals such as C-44300?
To be specific: is the arsenic component dangerous / carcinogenic? In case it is not, does it comply with FDA requirements for food service system?