1
will the retroactive reageing treatments used to enhance properties and prevent stress corrosion on aluminum zinc alloys be applicable to the aluminum copper alloys.
 
Replies continue below

Recommended for you

Not that I am aware of, at least as I understand your question. Re-ageing to prevent SCC is commonly applied to 7075-T6 and the resultant condition is designated T73. The copper aluminum alloys, such as 2014-T6 were develped to be SCC resistant in the T6 temper.
 